Butt Fusion welding checklist

Butt Fusion welding checklist

15/12/2020

Butt Fusion welding checklist
  • Trim the pipe ends all the way around
  • Clean the heater plates
  • When clamping the pipes in place, use the clamps to re-round the pipes
  • Correct procedure: Ask for evidence of recent, random weld inspections by your supervisors

Pressure

  1. Measure the drag pressure
  2. Check the right fusion pressure
  3. Add the two together for the overall pressure setting

Temperature

  1. Set the right heater place temperature (usually in the reange of 200-240C
  2. Give enough heat soak time for the pipe ends to fully heat up
  3. Keep dwell time down so the pipe ends don’t cool before contact

Alighnment

  1. Aim for less than 1mm misalignment
  2. For thicker pipes, misalignment must not exceed 10% of the pipe wall thickness (e.g. for 18mm thick pipe, no more thatn 1.8mm)

When you need focused help fast, get it from a supplier whose success is
keeping your plant moving. Call Advanced Piping Systems now on 1300 792 879

Related Articles

How drought popped this pipeline’s joints
Fittings

Are you thinking about replacing your existing pipeline with polyethylene? Well, here’s a story that you’ll find useful.  It’s a true story. It will show …

Quick guide: Poly Buttwelding Parameter Calculator (Single Low Pressure)

Buttwelding is the most common type of welding process used to join High-Density Polyethylene (HDPE) pipes and fittings. The process involves the joining of two …

Quick tips for successful electrofusion jointing of PE Pipe and fittings
Electrofusion Welding

One of the most common challenges we see in the field is ensuring successful electrofusion jointing of PE systems. Installations can be challenging, sometimes due …

Barcode interpretation for Electrofusion Poly Welding
Electrofusion Welding

This morning, we received an urgent call from a customer out on site who wanted to double-check the weld time for a 63mm electrofusion socket. …